Polymer Property : Shear Strength = 12.85 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 12.85 MPa
1864 psi
Lap
Epoxy Technology EPO-TEK® H35-175MPLV Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H35-175MPLV is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-el..