Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 38.6106 - 78.5 MPa

@Temperature 150 - 360 °C
5600.01 - 11400 psi

@Temperature 302 - 680 °F
Average value: 61.7 MPa Grade Count:6
Overview of materials for Polyimide
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Shear Strength 78.5 - 78.5 MPa

@Temperature 150 - 150 °C
11400 - 11400 psi

@Temperature 302 - 302 °F
Average value: 78.5 MPa Grade Count:1
Overview of materials for Thermoplastic Polyimide, Unfilled