Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 78.48 MPa @Temperature 23.0 °C |
11380 psi @Temperature 73.4 °F |
ASTM D732 |
Daelim H&L Plavis G15 Aromatic Polyimide, 15% Graphite Filled, Direct Formed
(Unverified Data**) Information provided by Daelim H&L |