Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 0.750 MPa | >= 109 psi | ISO 1922 |
3A Composites Core Materials AIREX® T92.100 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,.. |