Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1.85 MPa | 268 psi | average; ISO 1922 |
3A Composites Core Materials AIREX® T90.210 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has good mechanical properties and resistance to fatigue, is chemic.. |
|||
Shear Strength | 1.85 MPa | 269 psi | Overlap, Zinc (Galvanized), 50% RH |
3M 5200 Marine Adhesive/Sealant Fast Cure A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds with excellent adhesion to wood and fiberglass. Forms watertight, weather-resistant seals .. |
|||
Shear Strength | 1.85 MPa | 269 psi | Overlap, Fiberglass, 50% RH |
3M 5200 Marine Adhesive/Sealant Fast Cure A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds with excellent adhesion to wood and fiberglass. Forms watertight, weather-resistant seals .. |
|||
Shear Strength | 1.85 MPa | 268 psi | average; ISO 1922 |
3A Composites Core Materials AIREX® R63.140 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable.. |
|||
Shear Strength | 1.85 MPa | 269 psi | |
Dow Corning 3-0100 AUTOMOTIVE SEALANT One-part RTV, neutral cure, excellent unprimed adhesion, automotive oil resistant, and low volatilityInformation provided by Dow Corning |