Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1.80 MPa | 261 psi | ASTM C273 |
3A Composites Core Materials BALTEK® SB.50 Structural End-Grain Balsa BALTEK SB is a core material produced from certified kiln-dried balsa wood in the ‘end-grain’ confiation. It has extremely high strength and stiffness to weight ratios, and achieves an excellent b.. |
|||
Shear Strength | 1.80 MPa | 261 psi | ASTM C273 |
3A Composites Core Materials AIREX® PXw.385 Fiber-Reinforced Structural Foam Panel AIREX® PXw is a closed-cell, fiber reinforced polymer foam panel with a special formulation and very high mechanical properties. The sophisticated manufacturing process evenly distributes continuou.. |