Polymer Property : Shear Strength = 1.04 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength >= 1.04 MPa
>= 151 psi
Lap; ASTM D1002
Parker Chomerics CHO-BOND® 1016 Electrically Conductive Sealant
Description: CHO-BOND 1016 sealant is an electrically conductive, one-component RTV silicone which provides both environmental sealing and EMI shielding. This seal, filled with nickel-plated graphit..