Polymer Property : Shear Strength = 0.850 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.850 MPa
123 psi
average; ISO 1922
3A Composites Core Materials AIREX® C70.55 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..
Shear Strength 0.850 MPa
123 psi
Plate Shear, W direction
Hexcel® HexWeb® CRF-1/4-ACG-.002-3.4 Chromate free ACG® Honeycomb
Hexweb CRF is a hexagonal cell aluminum honeycomb material used principally as a shear carrying core in light weight adhesively bonded sandwich structures, and suitable for a wide range of other app..