Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.710 MPa | 103 psi | Cohesion Dynamic, PET/Stainless Steel; ASTM D1002 |
3M 7953MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Shear Strength | 0.710 MPa | 103 psi | Cohesion Dynamic, PET/Stainless Steel; ASTM D1002 |
3M 7956MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Shear Strength | 0.710 MPa | 103 psi | Cohesion Dynamic, PET/Stainless Steel; ASTM D1002 |
3M 9056MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |