Mechanical Properties Metric English Comments
Shear Strength 0.450 MPa
65.3 psi
ISO 1922
3A Composites Core Materials AIREX® C51.60 Industrial Processing Foam
AIREX® C51 is a closed-cell polymer foam with outstanding damage tolerance and formability. Its excellent price / performance ratio uniquely qualifies this core material for high-volume sandwich ..
Shear Strength 0.450 MPa
65.3 psi
Plate Shear, W direction
Hexcel® HexWeb® CRF-3/8-ACG-.002-2.3 Chromate free ACG® Honeycomb
Hexweb CRF is a hexagonal cell aluminum honeycomb material used principally as a shear carrying core in light weight adhesively bonded sandwich structures, and suitable for a wide range of other app..
Shear Strength 0.450 MPa
65.3 psi
average; ISO 1922
3A Composites Core Materials AIREX® C70.40 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..