Polymer Property : Shear Strength = 0.400 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength >= 0.400 MPa
>= 58.0 psi
ISO 1922
3A Composites Core Materials AIREX® T90.60 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..
Shear Strength 0.400 MPa
58.0 psi
Overlap, Maple, 50% RH
3M PN8017 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..
Shear Strength 0.400 MPa
58.0 psi
Overlap, Maple, 50% RH
3M PN8019 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..
Shear Strength 0.400 MPa
58.0 psi
Overlap, Maple, 50% RH
3M PN8027 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..
Shear Strength 0.400 MPa
58.0 psi
Overlap, Maple, 50% RH
3M PN8029 Marine Grade Silicone Sealant
A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b..
Shear Strength 0.400 MPa
58.0 psi
Plate Shear, W direction
Hexcel® HexWeb® CRF-3/4-ACG-.003-1.8 Chromate free ACG® Honeycomb
Hexweb CRF is a hexagonal cell aluminum honeycomb material used principally as a shear carrying core in light weight adhesively bonded sandwich structures, and suitable for a wide range of other app..