Mechanical Properties Metric English Comments
Shear Strength >= 0.200 MPa
>= 29.0 psi
ASTM C273
Parabeam Industrie Paraglass 12 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl..
Shear Strength 0.200 MPa
29.0 psi
Typical; ASTM C273
Parabeam Industrie Paraglass 12 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl..
Shear Strength 0.200 MPa
29.0 psi
Typical; ASTM C273
Parabeam Industrie Paraglass 15 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl..
Shear Strength 0.200 - 0.300 MPa
29.0 - 43.5 psi
Average value: 0.290 MPa Grade Count:5
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
Shear Strength 0.200 - 0.300 MPa
29.0 - 43.5 psi
Average value: 0.290 MPa Grade Count:5
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..
Shear Strength 0.200 MPa
29.0 psi
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Shear Strength >= 0.200 MPa
>= 29.0 psi
ASTM C273
Parabeam Industrie Paraglass 10 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl..