Polymer Property : 1% Secant Modulus = 62400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus 430 MPa
62400 psi
ASTM D790
ExxonMobil LL 5100.09 Compounding Resin
Product Description: LL 5100.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5100.09 makes for efficient blending ..