Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus | 294.2 MPa | 42670 psi | ASTM D638 |
Lotte Chemical Titan TITANEX® LI2516 Linear low density polyethylene resin
(discontinued **) LI2516 is a pelleted linear low density polyethylene with very narrow molecular weight distribution.Applications: House-wares, lids, closures and toys.Advantages: Excellent stress crack resistance,.. |