Mechanical Properties Metric English Comments
1% Secant Modulus 1280 MPa
186000 psi
Crosshead speed - 0.5" min; ASTM D790
LyondellBasell Alathon® M5350 High Density Polyethylene
ApplicationsALATHON M 5350 copolymer with narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing s..