Polymer Property : 1% Secant Modulus = 1370 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus 1370 MPa
198000 psi
Crosshead speed - 0.5" min; ASTM D790
LyondellBasell Alathon® M6028 High Density Polyethylene
ApplicationsM 6028 is a homopolymer that is warp resistant, exhibits excellent toughness, stiffness and color as well as low odor and good processing stability. Typical applications include safety ..