Polymer Property : 1% Secant Modulus = 131000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus 900 MPa
131000 psi
ASTM D638
SABIC M40053S High Density Polyethylene for Injection Molding
Product Description: M40053S is a UV stabilized high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to pro..