Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus | 1010 MPa | 146000 psi | Crosshead speed - 0.5" min; ASTM D790 |
LyondellBasell Alathon® M4621 High Density Polyethylene ApplicationsALATHON M 4621 is a copolymer that provides outstanding stress crack resistance and low temperature impact strength. Typical applications include small two-piece engine gas tanks, waste.. |