Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus | 689 MPa | 100000 psi | 0.5"/min; ASTM D790 |
LyondellBasell Petrothene® GA694189 Linear Low Density Polyethylene, Injection Molding Grade PETROTHENE GA694189 is a pelletized LLDPE copolymer resin for injection molding. Typical applications include lids and thin-walled items that require high flow and short cycle times. GA694189 exhibi.. |