Polymer Property : Dart Drop = 97.8 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 3.85 g/micron
97.8 g/mil
ISO 7765/1
Borealis Borstar® FB4250T LLDPE for Blown Film
Borstar FB4250 is well suited for a wide range of film applications due to its properties. The well balanced mechanical properties will improve the functionality of the films or allow for material ..