Mechanical Properties Metric English Comments
Dart Drop 3.66 g/micron
93.0 g/mil
ASTM D1709
Formosa Plastics Formolene® L62022B Film (Hexene Grade) LLDPE
Hexene Copolymer (Barefoot)Applications: Cast stretch film and high quality packaging films requiring clarity and toughness.A Hexene Copolymer Linear Low Density Polyethylene for film applications i..