Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 9.40 g/micron | 239 g/mil | F<sub>50</sub>; ASTM D 1709 |
Total PPH 3230 Polypropylene, Blow Molding Grade Homopolymer blow molding gradeLubricated - Fina 3230 offers superior core rod release, eliminating the need for additional lubricant.High Purity - Fina 3230 features minimum taste and odor and optim.. |
|||
Dart Drop | 9.40 g/micron | 239 g/mil | F<sub>50</sub>; ASTM D 1709 |
Total PPR 3230XZ Polypropylene, Blow Molding Grade Homopolymer Blow Molding GradeLubricated – FINA 3230XZ offers superior core road release, eliminating the need for additional lubricant.Antistat – FINA 3230XZ contains antistat to minimize dust ac.. |
|||
Dart Drop | 9.40 g/micron | 239 g/mil | F<sub>50</sub>; ASTM D 1709 |
Total PPR 8573 Polypropylene, Film Extrusion Grade Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8573 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The low m.. |
|||
Dart Drop | 9.40 g/micron | 239 g/mil | F<sub>50</sub>; ASTM D 1709 |
Total PPR 8473 Polypropylene, Film Extrusion Grade Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8473 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The very .. |
|||
Dart Drop | 9.40 g/micron | 239 g/mil | ASTM D1709B |
DuPont™ Surlyn® 2601 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 2601 is an ionomer resin available for use in blown and cast film operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins. Applicati.. |