Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 3.30 g/micron | 83.8 g/mil | F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Chevron Phillips 2151 High Impact, Liner Grade Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: High Impact Strength, Medium Slip, High Antiblock, Low Blocking and Good Openability, Good ProcessabilityApplications:Trash bags and other linersProcessing Co.. |
|||
Dart Drop | 3.30 g/micron | 83.8 g/mil | 1.5 in. dart/26 in. drop height; ASTM D 1709 |
Chevron Phillips HiD® 9632 HDPE Blown Film Resin
(discontinued **) Characteristics: Copolymerization Enhances Film Toughness, Excellent Film Drawdown Ideally Suited for Thin Films Production, Lower Melt Index (Higher Molecular Weight) Results in Increased Film Stre.. |
|||
Dart Drop | 3.30 g/micron | 83.8 g/mil | |
Dow LDPE 493A Low Density Polyethylene, Film Grade DOW LDPE 493A resin, is a high strength, general purpose resin used for shipping sack, industrial liner and produce film applications. DOW LDPE 493A resin can be blended with most linear low density.. |