Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 32.4 g/micron | 824 g/mil | ASTM D1709A |
ExxonMobil EXACT™ 4056 Plastomer for Film Blends and Blown Film Applications Product Description: Exact 4056 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin can be used in blends with polyolefins to improve.. |