Polymer Property : Dart Drop = 8.66 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 8.66 g/micron
220 g/mil
ASTM D1709
Westlake LF2020 Hexene Linear Low Density Polyethylene
Westlake LF2020 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s..
Dart Drop 8.66 g/micron
220 g/mil
ASTM D1709
ExxonMobil LD 317.09 Film Resin
LD 317 Series offer excellent impact strength, tensile properties, and heat sealability. Applications include ice bags, frozen food packaging, and other food packaging.Information provided by Exxon..
Dart Drop 8.66 g/micron
220 g/mil
ASTM D1709
ExxonMobil LD 317.87 Film Resin
LD 317 Series offer excellent impact strength, tensile properties, and heat sealability. Applications include ice bags, frozen food packaging, and other food packaging.Information provided by Exxon..