Polymer Property : Dart Drop = 750 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 29.5 g/micron
750 g/mil
ASTM D1709
Westlake Hifor Xtreme SC74844 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme SC74844 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip, high antiblock and processing aid. Films produce..
Dart Drop 29.5 g/micron
750 g/mil
ASTM D1709
Westlake Hifor Xtreme SC74853 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme SC74853 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains no slip, high antiblock and processing aid. Films produced wi..
Dart Drop 29.5 g/micron
750 g/mil
ASTM D1709
Westlake Hifor Xtreme SC74858 Linear Low Density Polyethylene
WESTLAKE HIFOR Xtreme SC74858 polymer is a high strength, good clarity linear low density polyethylene designed for blown film extrusion that contains no slip or antiblock and processing aid. Films ..