Polymer Property : Dart Drop = 73.3 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 2.89 g/micron
73.3 g/mil
ASTM D1709
Westlake EN1807AA Low Density Polyethylene
WESTLAKE polyethylene EN1807 is a fractional-melt low- density formulation suggested for film applications requiring high impact strength, high tear strength, and very good optical properties, such ..