Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 2.68 g/micron | 68.1 g/mil | at -18°C; ASTM D1709 |
Eastman Eastar A150 Copolyester, Film Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan.. |