Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 2.26 g/micron | 57.4 g/mil | ASTM D1709 |
Braskem HF 0144 HDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras.. |