Mechanical Properties Metric English Comments
Dart Drop 21.1 g/micron
536 g/mil
ASTM D1709A
ExxonMobil EXACT™ 3128 Plastomer for Blown Film Applications
Product Description: Exact 3128 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. It is designed fro both monolayer and multilayer coextruded ..