Polymer Property : Dart Drop = 35.6 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 1.40 g/micron
35.6 g/mil
F<sub>50</sub>; 1.5 in. dart/26 in. drop height; ASTM D 1709
Chevron Phillips 4610 LDPE High Clarity, Bakery Packaging Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: Excellent Clarity, Very High Gloss, Medium Slip, No Antiblock, Good Stability at High Drawdown Speeds, Good Printability, Good Heat Seal CharacteristicsApplic..
Dart Drop 1.40 g/micron
35.6 g/mil
1.5 in. dart/26 in. drop height; ASTM D 1709
Chevron Phillips HiD® 9662 HDPE Blown Film Resin  (discontinued **)
Resin Type: Linear Polyethylene HomopolymerCharacteristics: Unique Molecular Architecture Gives Outstanding Moisture Barrier Properties, Excellent Film Strength and Toughness for a Homopolymer, Give..
Dart Drop 1.40 g/micron
35.6 g/mil
F<sub>50</sub>; ASTM D 1709
Total PPR 6573XHC Polypropylene, Random Copolymer Film Grade
Random copolymer film gradeColor - Low catalyst residuals in FINA 6573XHC result in improved color stability.Clarity/Impact - The random copolymer structure of FINA 6573XHC improves its clarity and ..
Dart Drop 1.40 g/micron
35.6 g/mil
1.5 in. dart/26 in. drop height; ASTM D 1709
Chevron Phillips MarFlex® 9659 HDPE Blown Film Resin
Resin Type: Linear Polyethylene HomopolymerCharacteristics: Unique Molecular Architecture Gives Outstanding Moisture Barrier Properties, Excellent Film Strength and Toughness for a Homopolymer, Give..
Dart Drop 1.40 g/micron
35.6 g/mil
Dow LDPE 752A Low Density Polyethylene, Film Grade
DOW LDPE 752A resin is a drawdown film resin for thin gauge applications such as garment films. It contains high levels of both slip and antiblock additives. This material complies with U.S.FDA regu..