Mechanical Properties Metric English Comments
Dart Drop 11.8 - 13.4 g/micron
300 - 340 g/mil
ASTM D1709
BiologiQ ESR-PE EcoStarch mLLDPE Blend
Properties of 70% mLLDPE, 25% ESR, 5% additive blend - thin filmInformation provided by BiologiQ