Polymer Property : Dart Drop = 32.8 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 32.8 g/micron
833 g/mil
ASTM D1709
Braskem Flexus® 9210 LLDPE Blown Film Extrusion  (discontinued **)
25µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Automatic packaging (FFS); multilayer packaging films; films for lamination. Information provided by Braskem