Polymer Property : Dart Drop = 32.3 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 32.3 g/micron
820 g/mil
ASTM D1709
ExxonMobil Exceed™ 1012CA Film Resin  (discontinued **)
Exceed 1012CA mVLDPE resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1012CA resin have outstanding cold temperature toughness, impact strength a..