Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 3.95 g/micron | 100 g/mil | Calculated from thickness |
SIDPEC EGYPTENE® LL 0209 KJ LLDPE Film Applications:Refuse sacksProduce bags, carrier bagsFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o.. |
|||
Dart Drop | 3.95 g/micron | 100 g/mil | ASTM-D1709 |
Braskem Pluris 9300 LLDPE Blown Film Extrusion Polyethylene Quatropolymer Pluris 9300 is a Quatropolymer produced with Spherilene technology and is a LLDPE with unique properties, such as high stiffness associated with toughness. It is easier to process than conventional .. |