Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 3.42 g/micron | 86.9 g/mil | Calculated from thickness |
SIDPEC EGYPTENE® LL 0220 KJ LLDPE Film Applications: Light and medium duty film.Film properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor of Sidi Ke.. |