Polymer Property : Dart Drop = 3.41 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 3.41 g/micron
86.6 g/mil
ASTM D1709
ExxonMobil LD 103.MP Industrial Film Resin  (discontinued **)
LD 103 resins are homopolymer industrial film resins are used in box and drum liners, industrial packaging, medium duty shrink wrap, construction and agriculture film, and rubber bale wrap.Informati..