Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 0.600 - 2.70 g/micron | 15.2 - 68.6 g/mil | Average value: 1.54 g/micron Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Copolymer Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Copolymer Film Grade". Each property range of values reported is minim.. |