Dart Drop 6.563 g/micron
166.7 g/mil
ASTM D1709
ExxonMobil ESCOR™ AT 320 Cast Film Resin  (discontinued **)
ESCOR AT 320 provides excellent adhesion to a variety of substrates and other film components such as aluminum foil, polyolefins, polycarbonate, PET, etc.Information provided by ExxonMobil Chemical