Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 5.79 g/micron | 147 g/mil | ASTM D1709 |
Huntsman Rexell® L3103 Blown Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Excellent optics and sealability with good toughnessApplications: Stretch wrap and coextruded film for general packaging.FD.. |