Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop | 4.72 g/micron | 120 g/mil | ASTM D1709 |
Chevron Phillips MarFlex® 7109S LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Dart Drop | 4.72 g/micron | 120 g/mil | ASTM D1709 |
Huntsman PE1257 EVA Film Extrusion
(discontinued **) 2.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, good heat seal characteristics.Applications: Film extrusion: general purpose packaging where to.. |
|||
Dart Drop | 4.72 g/micron | 120 g/mil | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA967000 Low Density Polyethylene, Film Extrusion Grade Petrothene NA967000 is a low density polyethylene resin designed for blown film, general purpose and industrial packaging applications. NA967000 exhibits good processing characteristics and impact s.. |
|||
Dart Drop | 4.74 g/micron | 120 g/mil | Calculated from thickness |
SIDPEC EGYPTENE® LL 0205 AF LLDPE Film Applications:Heavy duty sacks, mulch filmsStretch film, liners, geomembraneFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l... |
|||
Dart Drop | 4.72 g/micron | 120 g/mil | ASTM D1709 |
Westlake LF1020 Butene Linear Low Density Polyethylene Westlake LF1020 is a butene LLDPE with excellent mechanical and downgauging advantages. It is suitable for can liners, stretch wrap, agricultural film, and blending with LDPE. This Kosher compliant .. |
|||
Dart Drop | 4.72 g/micron | 120 g/mil | ASTM D1709 |
Westlake LF1021 Butene Linear Low Density Polyethylene Westlake LF1021 is a butene LLDPE with excellent mechanical and downgauging advantages. It is suitable for can liners, stretch wrap, agricultural film, and blending with LDPE. This Kosher compliant .. |
|||
Dart Drop | 4.72 g/micron | 120 g/mil | ASTM D1709 |
Chevron Phillips MarFlex® 7109 LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Dart Drop | 4.72 g/micron | 120 g/mil | ASTM D1709 |
Chevron Phillips MarFlex® 7109DJ LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Dart Drop | 4.72 g/micron | 120 g/mil | ASTM D1709 |
ExxonMobil Pax-Plus™ 3204 Blown Film Resin Pax-Plus 3204 is a rubber modified high density polyethylene film resin which is used primarily in film requiring good impact strength. It is specially formulated to provide easy tear in the machin.. |