Polymer Property : Dart Drop = 1050 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 41.3 g/micron
1050 g/mil
ASTM D1709A
ExxonMobil EXACT™ 3131 Plastomer for Cast Film Applications
Product Description: Exact 3131 is an ethylene-based hexen plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3131 is designed for both monolayer and multilayer coex..