Polymer Property : Dart Drop = 0.890 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop 0.890 g/micron
22.6 g/mil
F 50; ASTM D1709/A
NOVA Chemicals Sclair® 19A Homopolymer HDPE Film Resin
Film Properties.Data provided by the manufacturer.
Dart Drop 0.890 - 30.0 g/micron
22.6 - 762 g/mil
Average value: 7.88 g/micron Grade Count:55
Overview of materials for High Density Polyethylene (HDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max..