Polymer Property : Elmendorf Tear Strength TD = 950 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 950 g
950 g
ASTM D1922
Huntsman Rexell® L8408 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, high quality blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength optics, and very low gel levels.Applications: Seali..
Elmendorf Tear Strength TD 950 g
950 g
ASTM D1922
Huntsman Rexell® L8101 Cast Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.Applications: Sealing layer in coextr..