Elmendorf Tear Strength TD 88 g
88 g
ASTM D1922
Dow DX5E66 Polypropylene Homopolymer Resin
OverviewConsistent processabilityVery high cleanlinessGood optical propertiesComplies with U.S. FDA 21 CFR 177.1520 (c)1.1a, EU-Directive 2002/72/EC, Canadian HPFB No ObjectionDX5E66 Developmental P..