Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 840 g | 840 g | ASTM D1922 |
ExxonMobil Escorene® LL-3023 LLDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3023 have outstanding tensile properties as well as stiffness and toughness.Applicatio.. |
|||
Elmendorf Tear Strength TD | 840 g | 840 g | Modified rectangular test specimen; ASTM D1922 |
Dow AFFINITY™ PL 1840G Polyolefin Plastomer (POP) AFFINITY™ PL 1840G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed to provide blown film with low temperature sealability, good puncture resistance, optics and.. |