Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 790 g | 790 g | |
Dow DOWLEX™ 2042A Linear Low Density Polyethylene, Food Grade DOWLEX® 2042A Polyethylene resin offers good tear strength, medium stiffness and outstanding toughness for films used in food contact applications. When used unmodified and processed according to g.. |
|||
Elmendorf Tear Strength TD | 790 g | 790 g | ASTM-D1922 |
Braskem Flexus® 9211 LLDPE Blow Film Extrusion Polyethylene Copolymer Braskem Flexus 9211 is a LLDPE hexene copolymer produced through a metallocene catalyst, which presents excellent impact and puncture strength beyond a differential sealing performance compared with.. |