Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 580 g | 580 g | ASTM D1922 |
ExxonMobil Enable™ 20-05HE Metallocene Polyethylene Resin Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Elmendorf Tear Strength TD | 580 g | 580 g | ASTM D1922 |
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Enable 20-05 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Elmendorf Tear Strength TD | 580 g | 580 g | ASTM D1922 |
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 20-05HH is a metallocene ethylene-hexene copolymer. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and p.. |
|||
Elmendorf Tear Strength TD | 580 g | 580 g | ASTM D1922 |
ExxonMobil Enable™ 20-05HE Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Enable 20-05 resins are metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Elmendorf Tear Strength TD | 580 g | 580 g | ASTM D1922 |
ExxonMobil Enable™ 20-05HH Metallocene Polyethylene Resin Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Elmendorf Tear Strength TD | 580 g | 580 g | ASTM D1922 |
ExxonMobil Enable™ 20-05CB Metallocene Polyethylene Resin Product Description: Enable 20-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |