Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 390 g
390 g
ASTM D1922
ExxonMobil Exceed™ 377D60 LDPE/Hexene Tough Premium Film Resin, 0.8 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 377D60 resin exhibit excellent impact strength and b..
Elmendorf Tear Strength TD 390 g
390 g
gF; ASTM D1922
Braskem LF0720/21AF Blown Film Extrusion Linear Low Density Polyethylene
Description: LF0720/21AF is a LLDPE Butene copolymer produced using Unipol® process technology. It shows low haze and high clarity associated with good balance of mechanical properties, processing ..