Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength TD | 328 g | 328 g | ASTM-D1922 |
Braskem LF 118/21 LLDPE Blown Film Extrusion Polyethylene Copolymer LF 118/21 is a LLDPE Butene copolymer produced by Braskem. It was specially designed to provide outstanding processing performance. Films obtained with this grade show good physical and optical prop.. |